The handheld 35RDC is a simple Go/No-Go ultrasonic instrument designed to detect subsurface defects caused by impact damage on solid laminate aircraft composite structures. The 35RDC features a backlit LCD that displays the word GOOD if no subsurface damage is found or the word BAD when it detects subsurface damage. It uses an ultrasonic transducer that can be placed or scanned on the area of composite material suspected of having impact damage. Weighing only 0.24 Kg (8.5 oz.)
and featuring a simplified keypad, this rugged ultrasonic instrument is easy to operate and requires minimal training.
Features
For use on solid laminate structure aerospace composites
Simple one-button calibration
Thickness range 0.63 mm to 22.8 mm (0.025 in. to 0.900 in.)
Advanced user setting shows A-scan or waveform. For use by qualified NDT personnel only.
General > Thickness Measurement Range**
0.63 mm to 22.8 mm (0.025 in. to 0.900 in.)
** Thickness range depends on material, transducer, and surface conditions.
General > Material Velocity
Fixed velocity for carbon fiber aerospace composite
General > Transducer Frequency
5.0 MHz
General > Measurement Update Rate
20 Hz
General > Deviation alarm set points
Programmable +/- from calibration point. Set in advance setup
Power Supply > Battery
3 AA alkaline or NiMH batteries
Power Supply > Operating Time
150 hours typical battery life; 30 hours continuous with backlight on
Power Supply > Low Battery Indicator
Continuously indicates battery status
Power Supply > Battery Saver
Auto Power Off/Continuous On
Power Supply > AC Power Supply
Optional
*This product is compliant to ROHS DIRECTIVE (EU) 2015/863, and the display contains less than 10 mg of mercury.
Optional Accessories
USB/ADP-115: AC-115 power supply
USB/ADP-230: AC-230 power supply
*All specifications are subject to change without notice.
Transducers
Olympus NDT offers a complete selection of transducers, cables, couplants, calibration test blocks, and accessories to meet a wide variety of ultrasonic precision thickness gaging applications.